Material : X2CrNi19-11
Steel number : 1.4306
Type : steel forged blind flanges
Standard : EN1092-1 Type 01
Grade : | X2CrNi19-11 | |||||||||||||||
Number: | 1.4306 | |||||||||||||||
Classification: | Austenitic stainless steel | |||||||||||||||
Density: | 7.9 g/cm ³ | |||||||||||||||
Standard: |
|
Particular ranges of sulphur content may provide improvement of
particular properties. For machinability a controlled sulphur
content of 0.015 % to 0.030% is recommended and permitted. For
weldability, a controlled sulphur content of 0.008 % to 0.030 % is
recommended and permitted. For polishability, a controlled sulphur
content of 0.015 % max is recommended. Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
C | Si | Mn | Ni | P | S | Cr | N |
max 0.03 | max 1 | max 2 | 10 - 12 | max 0.045 | max 0.015 | 18 - 20 | max 0.11 |
Rm - Tensile strength (MPa) (+A) | 460-700 |
Rm - Tensile strength (MPa) (+AT) | 460-680 |
Rm - Tensile strength (MPa) (+AT+C) | 740-780 |
Rp0.2 0.2% proof strength (MPa) (+AT) | 180 |
Rp0.2 0.2% proof strength (MPa) (+A) | 180-220 |
KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 60 |
KV - Impact energy (J) longitud., (+A) | +20° 100 |
A - Min. elongation at fracture (%) (+A) | 35-45 |
A - Min. elongation at fracture (%) longitud., (+AT) | 40 |
Nominal diameter (mm): | 2 - 50 |
Z - Reduction in cross section on fracture (%) | 63-68 |
Brinell hardness (HB): (+A) | 215 |
Brinell hardness (HB): (+AT) | 200 |
Resistance to intergranular corrosion: in the delivery condition -
yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -270 ° C |
EU EN | USA - | Japan JIS | France AFNOR | England BS | Italy UNI | Sweden SS | Poland PN | Finland SFS | Russia GOST | ||||||||||